Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3WG10 - PA6-GF50 - BASF

Material Data Center offers the following functions for Ultramid® B3WG10:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Glass fibre reinforced and heat ageing resistance injection moulding grade forindustrial parts requiring very high rigidity.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 22 / * cm³/10min ISO 1133
Température 275 / * °C -
Charge 5 / * kg -
Retrait au moulage, parallèle 0.2 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 16000 / 11000 MPa ISO 527
Contrainte à la rupture 235 / 160 MPa ISO 527
Déformation à la rupture 3 / 5.5 % ISO 527
Module de fluage en traction, 1h * / 9600 MPa ISO 899-1
Module de fluage en traction, 1000h * / 7400 MPa ISO 899-1
Résistance au choc Charpy, +23°C 100 / 110 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 90 / 98 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 22 / 30 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 16 / 13.3 kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 220 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 215 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 220 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 220 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 15 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 73 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Yellow Card disponible oui / * - -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Yellow Card disponible oui / * - -
Aptitude à l'allumage 22.5 / * % ISO 4589-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 1MHz 4.2 / 6.1 - IEC 62631-2-1
Facteur de pertes, 100Hz 140 / 1400 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 140 / 1400 E-4 IEC 62631-2-1
Résistivité transversale 1E13 / 1E10 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 1E10 Ohm IEC 62631-3-2
Rigidité diélectrique 40 / 31 kV/mm IEC 60243-1
Indice de résistance au cheminement - / 450 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 4.8 / * % Sim. to ISO 62
Absorption d'humidité 1.5 / * % Sim. to ISO 62
Masse volumique 1550 / - kg/m³ ISO 1183
Propriétés spécifiques à la matièresec / condUnitéNorme du test
ISO Data
Indice de viscosité 135 / * cm³/g ISO 307, 1157, 1628
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 300 °C ISO 294
Injection, température du moule 80 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 4 h -
L'humidité de traitement ≤0.15 % -
Température de la matière fondue 280 - 300 °C -
Température du moule 80 - 90 °C -
Fonctions
Module de cisaillement dynamique / Température , Ultramid® B3WG10 (sec), PA6-GF50, BASF
Module de cisaillement dynamique / Température , Ultramid® B3WG10 (cond.), PA6-GF50, BASF
Contrainte / Déformation , Ultramid® B3WG10 (sec), PA6-GF50, BASF
Contrainte / Déformation , Ultramid® B3WG10 (cond.), PA6-GF50, BASF
Module sécant / Déformation , Ultramid® B3WG10 (sec), PA6-GF50, BASF
Module sécant / Déformation , Ultramid® B3WG10 (cond.), PA6-GF50, BASF
Contrainte / Déformation (isochrone) 23°C, Ultramid® B3WG10 (cond.), PA6-GF50, BASF
Module de fluage / Temps 23°C, Ultramid® B3WG10 (cond.), PA6-GF50, BASF
Courbe de fluage 23°C, Ultramid® B3WG10 (cond.), PA6-GF50, BASF
Contrainte / Déformation (isochrone) 60°C, Ultramid® B3WG10 (sec), PA6-GF50, BASF
Module de fluage / Temps 60°C, Ultramid® B3WG10 (sec), PA6-GF50, BASF
Courbe de fluage 60°C, Ultramid® B3WG10 (sec), PA6-GF50, BASF
Contrainte / Déformation (isochrone) 90°C, Ultramid® B3WG10 (sec), PA6-GF50, BASF
Module de fluage / Temps 90°C, Ultramid® B3WG10 (sec), PA6-GF50, BASF
Courbe de fluage 90°C, Ultramid® B3WG10 (sec), PA6-GF50, BASF
Contrainte / Déformation (isochrone) 120°C, Ultramid® B3WG10 (sec), PA6-GF50, BASF
Module de fluage / Temps 120°C, Ultramid® B3WG10 (sec), PA6-GF50, BASF
Courbe de fluage 120°C, Ultramid® B3WG10 (sec), PA6-GF50, BASF
Module de traction / Température , Ultramid® B3WG10 (sec), PA6-GF50, BASF
Module de traction / Température , Ultramid® B3WG10 (cond.), PA6-GF50, BASF
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Lubrifiant, Agent de démoulage
Propriétés spéciales
Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 300 °C
injection molding, Melt temperature, recommended: 290 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.